SAN Graphite/Glass
SAN Graphite/Glass
North America
SDS - Safety Data Sheet
PSB - Product Stewardship Bulletin
Melt Flow Rate | 2.0 to 15 g/10 min |
Density - Specific Gravity (Method A) | 1.28 to 1.33 g/cm³ |
Tensile Strength at Yield (5.0 mm/min, 23 °C, Type I) | 48.3 MPa |
Flexural Modulus (1.3 mm/min, 23 °C, Procedure A, Method I (3 point load), Type I) | 6900 MPa |
Notched Izod Impact (23 °C, Method A) | 21 J/m |
Drying Time | 2.0 to 4.0 hr |
Drying Temperature | 82 °C |
Processing (Melt) Temp | 199 to 282 °C |
Injection Rate | Moderate-Fast |
Mold Temperature | 60 °C |
Injection Molding