Density |
1.26 g/cm³ |
Density - Specific Gravity |
1.26 g/cm³ |
Change in Volume (in Reference Fuel B, 27 °C, 168 hr) |
29 % |
Change in Volume (in Reference Fuel B, 27 °C, 168 hr) |
29 % |
Change in Volume (in ASTM #1 Oil, 100 °C, 168 hr) |
-14 % |
Change in Volume (in ASTM #1 Oil, 100 °C, 168 hr) |
-14 % |
Change in Volume (in IRM 903 Oil, 100 °C, 168 hr) |
23 % |
Change in Volume (in IRM 903 Oil, 100 °C, 168 hr) |
23 % |
Change in Volume (in Water, 100 °C, 168 hr) |
8.0 % |
Change in Volume (in Water, 100 °C, 168 hr) |
8.0 % |
Melt Viscosity (190 °C, 300 sec^-1) |
640 Pa·s |
Tensile Stress at 100% (1.90 mm) |
5.30 MPa |
Tensile Stress at 100% (1.90 mm) |
5.30 MPa |
Tensile Stress at 100% (125 °C, 1.90 mm) |
4.40 MPa |
Tensile Stress at 100% (125 °C, 1.90 mm) |
4.40 MPa |
Torsion Modulus (24 °C, 1.9 mm) |
2.9 MPa |
Torsion Modulus (-20 °C, 1.9 mm) |
14.3 MPa |
Tensile Set |
11 % |
Clash-Berg Modulus (-32 °C) |
68.9 MPa |
Tensile Strength at Yield (1.90 mm) |
9.90 MPa |
Tensile Strength at Yield (125 °C, 1.90 mm) |
5.50 MPa |
Tensile Stress at Yield (1.90 mm) |
9.90 MPa |
Tensile Stress at Yield (125 °C, 1.90 mm) |
5.50 MPa |
Tensile Strain at Break (1.90 mm) |
400 % |
Tensile Strain at Break (125 °C, 1.90 mm) |
140 % |
Tensile Elongation at Break (125 °C, 1.90 mm) |
140 % |
Tensile Elongation at Break (1.90 mm) |
400 % |
Tear Strength (Die C, 1.90 mm) |
33.3 kN/m |
Ductile/Brittle Transition Temperature |
-76 °C |
Ductile/Brittle Transition Temperature |
-76 °C |
Change in Shore Hardness in Air (Shore A, 125 °C, 168 hr) |
-5.0 |
Shore Hardness (Shore A, 1.90 mm, Compression Molded) |
76 |
Change in Durometer Hardness in Air (Shore A, 125 °C, 168 hr) |
-5.0 |
Durometer Hardness (Shore A, 1.90 mm, Compression Molded) |
76 |
Compression Set (24 °C, 22 hr, Method B) |
17 % |
Compression Set (100 °C, 22 hr, Method B) |
61 % |
Compression Set (24 °C, 22 hr) |
17 % |
Compression Set (100 °C, 22 hr) |
61 % |
Taber Abrasion Resistance (CS-17 Wheel, 1000 g, 1000 Cycles) |
10.0 mg |
Processing (Melt) Temp |
177 °C |